http://rdf.ncbi.nlm.nih.gov/pubchem/patent/SU-1661145-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_25d0e99dc8221a6651135cb29b74184b |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B39-04 |
filingDate | 1989-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1991-07-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b04a2852b6d559649e8e399335514dbf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f1fa7b4ac249b7a95f3ddcbb838ff186 |
publicationDate | 1991-07-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | SU-1661145-A1 |
titleOfInvention | Method for ceolite eu-2 preparation |
abstract | The invention relates to methods for producing zeolite EU = 2, used as an adsorbent and catalyst in the processing of petroleum synthesis products, and reduces the cost of the product while maintaining its high adsorption properties, as well as simplify the process. The SIO 2 sol and ethylenediamine (EDA) solution in water are mixed at the following molar ratios H 2 O: SIO 2 = 15-5 and EDA: SIO 2 = 0.5-5.0. The mixture is subjected to hydrothermal crystallization in an autoclave at 220 ° C for 12 hours. The crystalline precipitate obtained is separated from the mother liquor, washed, dried and calcined. 2 tab. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2527283-C2 |
priorityDate | 1989-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 23.