http://rdf.ncbi.nlm.nih.gov/pubchem/patent/SU-1616933-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e5f3db1b2456dfee2389f5b541f5d463 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-43 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 |
filingDate | 1988-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1990-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a0ac08f8980a36372e4d4b3bee9b4510 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f189012983a5bd7b199221936ada46e8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_031f9a14103c23a8f4d08b5ac6f9999d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dc602bf90111c2c54124328430852813 |
publicationDate | 1990-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | SU-1616933-A1 |
titleOfInvention | Vulcanizable rubber mix |
abstract | The invention relates to the tire industry, in particular to the development of a rubber compounding for the manufacture of tread rubber of large-sized car tires. The invention allows to increase the resistance to repeated stretching rubbers (deformation of 150%) after heat aging (100 ° C. For 72 hours) to 39 thousand. Cycles through the use of the rubber composition of one of the substances selected from the group consisting of di- (2-benzothiazolyl ) disulfide, tetramethylthiuram disulfide, alkilfenoldisulfidnuyu resin having a softening point of 110-130 ° C and a sulfur content of 29,3-31,8 wt.%, or N, N-1 th fenilenbismaleinimida in combination with di- (2-benzothiazolyl) disulfide in mass ratio (1-3): 0.4. The composition contains, by weight.h .: natural cis-1,4-polyisoprene rubber 70n n n synthetic cis-1,4-polyisoprene rubber 30n n n sulfur 0.5-1.5n n n N-cyclohexylbenzothiazole sulfenamide-2 or (benzothiazolyl-2) -morpholine sulfide 0.01-1.5n n n N, N 1 -dithiodimorpholine 0.01-2.0n n n zinc oxide 3.0-6.0n n n stearic acid 1-3n n n 1-3 sodium stearinaten n n Melt hexachloroparaxylene in a wax mixture in a mass ratio (80-85): (15-20) 0.3-1.0n n n phthalic anhydride or N- (cyclohexylthio) phthalimide 0.1-0.7n n n rosin 1-4n n n aromatic petroleum oil 0.01-11.0n n n N-isopropyl-N 1 -phenylphenylenediamine-1,4 or N- (1,3-dimethylbutyl) -N 1 -phenylphenylene diamine-1,4 0.5-3.0n n n 2,2,4-trimethyl-1,2-dihydroquinoline oligomer 1-3, silica filler 5-15n n n carbon black 40-60n n n di- (2-benzothiazolyl) disulfide 0.1-0.6 or tetramethylthiuram disulfide 0.1-0.5, or the indicated alkylphenol disulfide resin 1-3, or N, N 1 -m-phenylene bismaleimide in combination with di- (2- benzothiazolyl) disulfide in a mass ratio of (1-3): 0.4 1.4-3.4. 2 tab. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6171517-B1 |
priorityDate | 1988-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 77.