http://rdf.ncbi.nlm.nih.gov/pubchem/patent/SU-1461397-A1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4ccec37b5e0b8ab71cf050dfc38e7345
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A23K1-10
filingDate 1985-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date>
grantDate 1989-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_95c25e60539a7b6787b72d26c79d549e
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_af63ea1f16a288e9f773791e9512abe8
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_465cf7b9c5fa6279f54b2134fdac82e0
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_93904e0ea2eb387179facb92624fe523
publicationDate 1989-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber SU-1461397-A1
titleOfInvention Method of processing waste of animal origin
abstract The invention relates to the production of feed additives from animal waste. The purpose of the invention is to reduce the duration of the process and reduce the loss of nutrients. Feed additives are obtained; in natural gas boilers, natural zeolite, previously made up to particles of 0.5–3.0 mm in size and heated to 150–200 ° C, and waste of animal origin, are fed into vacuum boilers; intermittently to dry the mixture until the relative humidity of the resulting mass reaches 40-55% and the zeolite content in the final product is 10-40% of the total mass, after which the product is finally dried. At the same time, the total time for waste processing is reduced to 3.4 hours and the lost nutrients are reduced by reducing the amount of fluids in the finished product (C (L
priorityDate 1985-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID414859283
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID6547

Total number of triples: 16.