Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f51e23611621a91a7a7bae4256581b44 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B25-14 |
filingDate |
1985-08-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1988-04-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_688f1a9cba30b0b760772dd93e172bf3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_42a46ea7fcde266f836afe56ab52b7ee http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d3d6004dcdd51d96226add155edd89cd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6243c3c3e8ba6cc1af97bc0bcb634eb0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bced04ac0abc0ebedae829e73e3efa59 |
publicationDate |
1988-04-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
SU-1386559-A1 |
titleOfInvention |
Method of producing modified phosphorus pentasulfide |
abstract |
The invention relates to the technology of producing high phosphorous phosphorus with high reactivity. The aim of the invention is to increase the reactivity of the product. The method consists in melting the melt, phosphorous phosphate for 1-5 hours in an inert gas containing 1.0-2.5% by volume of oxygen, dividing the melt into the upper and lower parts, followed by separate crystallization of them in a flaking machine. 1 tab. |