http://rdf.ncbi.nlm.nih.gov/pubchem/patent/SU-1298217-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d82b3f07bf79a17ec1cd780c053a96bd |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 |
filingDate | 1984-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1987-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1d95a304de165b140775cacc33478a8d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6e45a4d1aa3d6eb83653b42a4b3f24ca http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5acb3b98f660338867dfd075b5ed227e |
publicationDate | 1987-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | SU-1298217-A1 |
titleOfInvention | Butadiene-methylstyrene rubber-base stock |
abstract | This invention relates to the preparation of styrene-butadiene rubber based rubber compounds. The invention makes it possible to increase the resistance to heat aging and the strength properties of rubber by using a complex based on poly (ethylene polyamine and copper chloride) in the rubber mixture as antioxidants. The rubber mixture contains.: Butadiene methyl styrene rubber 100, stearic acid 0.5-1.5; zinc oxide 3.0-5; di (2-benzothiazolyl) disulfide 0.5-2.5; carbon black 40-50, sulfur 2-3 and complex 2-4. 13 tab. (L N3 WITH QO to |