http://rdf.ncbi.nlm.nih.gov/pubchem/patent/SU-1121284-A1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_054880d159f23d3d301f63f6c1e70306
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d0e5fa3f160fe9f7cf62d39d75f683c1
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_532138e15b5012bcae86eb580fdec8f7
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_94820c74c5f000b58800981fedc33ef4
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_585148c5e68bf52a29814c07ee6c4a3f
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dcfe76d335f19dbbd5ca468fe978e23c
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10G73-36
filingDate 1982-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date>
grantDate 1984-10-30-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7ff3c249b42bd471233d3e46b4d13e54
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ac2bde55b57bfd9767428d2c15e26536
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_78dced19a68862c4cfc86d1297315627
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3cfcd6ed0e73602af21e68f7d1b602d8
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cec931b0eb1f9bccf3b03493121043e1
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_53d92d576355825d6c6679c645d0daa1
publicationDate 1984-10-30-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber SU-1121284-A1
titleOfInvention Method for producing plastic paraffins
abstract A METHOD FOR OBTAINING PLASTIC PARAFINS by de-oiling the petroleum fractions boiling at 280470 0 in the presence of a selective solvent upon cooling. and step-by-step filtration with the release of paraffin wax with a melting point of 50-55 ° C and an oil content of 6.5-2.3%, followed by dewaxing of the first-stage filtrate solution to produce deparate-rich oil and low-melting slack, characterized in that properties of paraffin and increase in its code, low-melting slack are additionally deoiled with selective solvents in conditions of obtaining low-melting plastic paraffin with a melting point of 37-45 ° C and content of crystallizing . Isomeric hydrocarbon cyclic structure and 20-35 wt%, and the resulting plastic paraffin wax is mixed with paraffin wax in a weight ratio of 10: 90-90: 10.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-9628522-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10738248-B2
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2693173-C9
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2693173-C1
priorityDate 1982-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419595960
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID11262

Total number of triples: 27.