http://rdf.ncbi.nlm.nih.gov/pubchem/patent/SU-1109487-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_71b544ab14d033da9555c315b2655ecf |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-564 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-46 |
filingDate | 1982-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1984-08-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_43054be2d8b342ffba029222a82c91f5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3eff10b0f057702001e6b457adcacdc0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_de7ebe6d8b27e34f0ba59999ac5a0630 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dfe0ae5679393bc71748b57727a87922 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e2359ae144e2299d846b4e40f7f4bc02 |
publicationDate | 1984-08-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | SU-1109487-A1 |
titleOfInvention | Process for making clothes of flax and flax-cotton mix uncrumpled in wet condition |
abstract | METHOD OF ADDING TISSUES FROM FLAX AND MIXTURE HIM WITH COTTON INSTRUMENTS COLORED COLORING COLORING PATIENTS IN WETTING STATE By impregnating a fabric with a composition containing quaternary ammonium salt of bis- (diethylaminomethyl) ethylene urea, polyethylene emulsion, urea, hexaqem, ancillary gene, urea, hexahydrate, ethylene urea, polyethylene emulsion, urea, hexaigrade, and other characterized in that, in order to increase the strength characteristics of the tissues, the impregnation is carried out with a composition containing an additional preparation epamin-06 based on the condensation product of epichlorohydrin with polyethylene glycol and diethylenetriamine in the following ratio of components, g / l: The drug epamin-06 per dry BeniecTBO36-44. Quaternary ammonium salt of bis (diethyl (L aminomethyl) ethylene urea 75-100 Polyethylene emulsion based on dry matter substance 2-3 Urea 8-10 Hexahydrate about 4 magnesium chloride 10-15 Water Others up to 1 l, x and after heat treatment, the fabric is further treated in water caustic soda solution with a concentration of 40-60 g / l. |
priorityDate | 1982-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |