http://rdf.ncbi.nlm.nih.gov/pubchem/patent/SU-1011052-A3
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d44b532d6aa1bf173c57dad794450202 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-043 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L15-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L17-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L89-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L15-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02C7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L17-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08H1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L17-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08H1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L89-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L27-22 |
filingDate | 1979-10-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1983-04-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f88b50d936ca23562408397ba26fe2a7 |
publicationDate | 1983-04-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | SU-1011052-A3 |
titleOfInvention | Process for preparing hydrogel |
abstract | 1. Process for the preparation of a three-dimensional structure, characterized in that it consists in forming an acid aqueous solution of a natural, non-crystalline protein polymer of animal or plant origin, or of a mixture of such polymers, these polymers having low molecular weights of not more than 100 000, in heating the solution to a temperature between 55 and 65 degrees C, in adjusting the pH of the solution to between 3.5 and 5.5, in adding a crosslinking agent to the solution and incorporating it therein, in a ratio of 0.5 % to 15 % by weight, the temperature of the solution being kept at between 55 and 65 degrees C, in drying the solution until its moisture content does not exceed 10 % at a maximum temperature of 35 degrees C or an equivalent temperature in vacuo, so as to form a crosslinked polymeric structure, in subjecting this structure to thorough washing with water, in subjecting the structure washed in this way to dehydration by immersion in a water-miscible organic solvent, in subjecting the structure to thorough washing with water, and in drying the structure again at a maximum temperature of 35 degrees C, until its moisture content does not exceed 10 %. |