Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_122e7323d555493f1ff7477b3e55286a |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H25-00 |
filingDate |
2005-07-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_da4af682434a11c8000dc8aafcb1e74e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d7429204e7f6fc3d9190dea34e4184c3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ce2ae95017e0a64e6a8ffd386c33bdac http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_65a0cd9058c60c2d3affd6d895aa3121 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bb9b9f5171166d7b781d0a27bad7ebec http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7deb439d73520de30b99061cb9b44dfc |
publicationDate |
2010-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
SK-5527-Y1 |
titleOfInvention |
Prearation for deacidification and ensuing rise of solidity and stability of paper information carrier and method for using thereof |
abstract |
It is described an aqueous solution of zirconium compounds, consisting of zirconate-potassium carbonate with a concentration the most 6 % by weight and containing an addition of water-soluble polysaccharide compounds with a concentration the most 2 % by weight. The said solution is coated or sprayed to information paper carriers for the most 30 min. at room temperature. Thus, the treated information paper carriers are further dried and pressed at room temperature, if it is necessary. |