http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2764926-C1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_839410b0756315dc9834bf1b49268705 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K3-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K3-00 |
filingDate | 2021-04-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6d74fd22d662d6f28947d3b7b453596d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_20087bff57fde0627973ccb0b34ccbc9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a3b1a2bb4650f89f9e64cd24426c9400 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e94002be88556b37a8cd3ff33417c6ee http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b9c1a77d4b4d833e2ea1af385a2e2776 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bdb8ac3ebcd58bbac67b5ae3320978e6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_02b18eee4c709ed3aa7fb796b819e2b2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8b7ad423ab75520829901d30649e7ad8 |
publicationDate | 2022-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2764926-C1 |
titleOfInvention | Wood modification method |
abstract | FIELD: woodworking industry.SUBSTANCE: invention relates to the woodworking industry, in particular to the production of treated wood to increase its water resistance. Wood is processed by the immersion method in an impregnating solution under normal conditions, followed by heat treatment. In this case, 3% of the mass is used as the impregnating solution. a solution of a previously obtained copolymer of glycidyl methacrylate and hexyl methacrylate, decyl methacrylate, lauryl methacrylate, tetradecyl methacrylate, stearyl methacrylate derivative of methacrylate in methyl ethyl ketone, with a molar ratio of monomers equal to (4-1.5):1. The impregnation is carried out for 2 hours, and the heat treatment is carried out at 140°C for 2 hours.EFFECT: process of wood hydrophobization is simplified and its water resistance is increased.1 cl, 4 dwg, 1 tbl |