http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2687899-C2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3fbc0909ebea3ec19d4afa35b8fce91c |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P20-143 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10C3-002 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10C3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J11-02 |
filingDate | 2018-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fca8c141366a9f6fbbc7d8684bb9cfc6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_923c6df7a6dee3963223675310291505 |
publicationDate | 2019-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2687899-C2 |
titleOfInvention | Method of producing pitch from waste fractionation of still residue of styrene |
abstract | FIELD: technological processes.SUBSTANCE: invention relates to processing coal-tar pitch and is intended for increasing its output due to combined processing of rectification wastes of styrene and coal-tar pitch. During combined processing, which is carried out at temperature of 350–380 °C, obtaining high-temperature pitch with temperature softening T>100 °C, fuel oil and gas products.EFFECT: raw material base for producing coal-tar pitch is expanded, and still residues of rectification of styrene are utilized.1 cl, 3 ex |
priorityDate | 2018-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |