http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2631324-C2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5b0b27593c8d7ab779766afe5ba89d3c |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2031-324 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2077-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G69-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-2855 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2007-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-003 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G69-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G69-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-003 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G69-18 |
filingDate | 2013-03-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d36eebc1fa87ca68c544151ed17e1d2d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a6fbbba9c143b0442bdc94b199f5e45a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9df026e5408fd01a831c059585ea1bcd |
publicationDate | 2017-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2631324-C2 |
titleOfInvention | Moulded polyamides, method of their production and their application |
abstract | FIELD: chemistry. n SUBSTANCE: method for producing a moulded polyamide consists in that, at least, one lactam melt with an anionic polymerization catalyst and optionally a tertiary amine co-activator and/or dibutyltin dilaurate is mixed with, at least, one lactam melt with a biuret polymerization activator or uretdione, and, if necessary, the aforementioned co-activator. The polymerization is then carried out in a mould at a temperature of, at least, 80°C to 130°C, preferably of 110°C to 130°C. Herewith the co-activator must be contained in, at least, one of the lactam melts. If necessary, a lactam melt with a co-activator can be introduced before polymerization. The moulded polyamide is used to make rollers, preferably for passenger elevators, and preforms, preferably containers, gears, tubes, rods and plates for engineering and the automotive industry. n EFFECT: invention makes it possible to produce polyamides with a short holding time produced at low temperatures, as well as to produce moulded parts with improved characteristics. n 7 cl, 1 tbl, 1 ex |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2697332-C1 |
priorityDate | 2012-05-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 103.