Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bda0bdf40297a2c29891902e7d6053fb |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2203-142 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2203-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2361-14 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-141 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G8-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L61-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G8-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-144 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G10K11-162 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K21-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G8-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G8-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G8-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16L59-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G8-34 |
filingDate |
2012-11-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2016-03-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_87abfd21f209d22a0b7228c4b49dd42d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_71dae05e5338fe95b7994e07be0b38b9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9e5a371f0ea6c178d718e7c76eae5ffc |
publicationDate |
2016-03-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
RU-2577378-C2 |
titleOfInvention |
Foam plastic based on phenol resins |
abstract |
FIELD: chemistry. n SUBSTANCE: invention relates to a foam-based phenolic resins and use thereof. Foam is produced by using at least following steps: a) production of a prepolymer by condensing at least a phenol compound and formaldehyde in a ratio of 1:1.0-1:0.15-5 using 3.0 wt% of raw materials used a basic catalyst at a temperature from 50 to 100°C to obtain refractive index of reaction mixture of 1.4990-1.5020 measured at 25°C according to DIN 51423-2; b) addition of 5 to 40 wt% of raw materials used by at least one natural polyphenol at a temperature of 50 to 100 °C; c) addition of 2 to 10 wt% of feedstock used one or more emulsifiers, and mixtures thereof; g) addition of 2 to 10 wt% of feedstock used one or more blowing agents, and mixtures thereof; d) addition of 10 to 20 wt% of raw materials used hardener and e) curing. n EFFECT: result is production of biological material based on a thermosetting foam having improved properties, in particular enhanced fire retardant properties with substantially constant properties of foam. n 10 cl, 6 ex |