abstract |
FIELD: chemistry. n SUBSTANCE: method of obtaining a composite material includes the influence on a mixture of a carbon-containing material, filler and sulphur-containing compound by a pressure of 0.1-20 GPa and a temperature of 600-2000°C. As the sulphur-containing compound applied is carbon bisulphide, a compound from the mercaptan group or a product of its interaction with elementary sulphur. As the carbon-containing material applied is molecular fullerene C60 or fullerene-containing soot. As the filler applied are carbon fibres, or diamond, or nitrides, or carbides, or borides, or oxides in the quantity from 1 to 99 wt % of the weight of the carbon-containing material. n EFFECT: obtained composite material can be applied for manufacturing products with the characteristic size of 1-100 cm and is characterised by high strength, low density, solidity not less than 10 GPa and high heat resistance in the air. n 11 cl, 3 dwg, 11 ex |