http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2545541-C2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7dfdebf3f399cea1df09087a5cc60716 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2495 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A41D19-0082 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C41-003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C41-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A41D19-0058 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-02 |
filingDate | 2005-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-04-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5ad1925e49733f43115fb438d85403a9 |
publicationDate | 2015-04-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2545541-C2 |
titleOfInvention | Elastomeric films and gloves |
abstract | FIELD: chemistry. n SUBSTANCE: invention relates to a method and a composition for manufacturing a multi-layered elastomeric film, suitable for gloves. The composition for manufacturing the elastomeric film contains a synthetic elastic polymer or a copolymer. The total concentration of solid substances in the composition constitutes 5-20 wt % of the composition weight. The method of manufacturing the elastomeric film with the application of a multi-layered coating contains the following stages: (i) dipping the mould into a coagulant with the content of calcium ions and concentration of 1-10 wt %; (ii) drying the dipped mould; (iii) dipping the mould into the composition for the elastomeric film manufacturing with the temperature of 25-45°C with a 1-10 s exposure; (iv) drying the elastomeric film composition; (v) re- dipping the mould into the composition for the application of the next layer of the elastomeric composition; (vi) optional repetition of stages (iv) and (v); (vii) drying and vulcanisation of the multi-layered elastomeric film with the average layer thickness from 6 to 90% of the average total thickness of the multi-layered film, and the average total thickness of the multilayered elastomeric film from 0.01 to 0.3 mm. n EFFECT: invention makes it possible to increase the strength of the finished film without defects, does not cause skin allergy. n 12 cl, 10 tbl, 2 ex |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10925335-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11559090-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2724256-C2 |
priorityDate | 2005-07-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 67.