Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_023f8ee60cbed3d604e18deaeb3957df |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B11-26 |
filingDate |
2013-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2015-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_43eb19af3fd29679fceed6cecfa11959 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0144dc7d58aff09324aa7f9e16f84999 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d45dc8b08fed31f14e2feee4c8dad6b2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eef2100496bee30d3126967aa74768dd |
publicationDate |
2015-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
RU-2540706-C1 |
titleOfInvention |
Binding agent |
abstract |
FIELD: chemistry. n SUBSTANCE: binding agent contains components with the following ratio, wt %: phosphogypsum dehydrate - 77.0-87.5; silica-containing component of technogenic origin - finely disperse broken ceramic bricks (FDCB) or haydite dust from cyclones (HD) - 10.0-20.0; zinc stearate - 2.5-3.0. n EFFECT: increase strength and water resistance of the material. n 4 tbl |