http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2540306-C1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1cf2e7934165c16d2f640a32de76e87a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D149-00 |
filingDate | 2013-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_505e7b32b729300f8efe99f9c0d4c7fb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_92c490e3ce32d253340f0fbfdb36dd97 |
publicationDate | 2015-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2540306-C1 |
titleOfInvention | Method of accelerating solidification of polymer coatings based on ethynol varnish |
abstract | FIELD: chemistry. n SUBSTANCE: invention relates to methods of anticorrosion and hydroinsulation protection of building constructions and structures and can be used for acceleration of solidification of polymer coatings based on divinylacetyl varnish - ethynol varnish Method of accelerating solidification of polymer composition based on ethynol varnish includes blowing non-solidified polymer composition based on ethynol varnish, including ethynol varnish, expanded clay dust and divinylstyrene latex SKS-65, with its mixing for 20-40 minutes by intensive flows of compressed oxygen before application of coating on the surface to be protected and its natural solidification at the environment temperature. n EFFECT: invention makes it possible to reduce time of complete solidification of polymer coatings of compositions based on ethynol varnish in wide range of temperatures. n 1 ex |
priorityDate | 2013-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 28.