http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2519158-C1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3e4a5c4b968ccc07b753af1001e2aec2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L15-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L15-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L15-32 |
filingDate | 2013-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-06-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5d25da057bc2f8e93823dd703e5b3929 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_95c0fd43c833a3e07b9a35e257ff643f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_da841a06008c83b9bae06411302e22d3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9b403bd0e0e7ca8bf274823a7535b24a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dd05c347e8d853f9e798b0acf861aeea |
publicationDate | 2014-06-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2519158-C1 |
titleOfInvention | Biodegradable wound coating and method for preparing biodegradable wound coating |
abstract | FIELD: medicine. n SUBSTANCE: what is described is a coating in the form of a film which contains the following ingredients, wt %: low-molecular edible chitosan 5.3-5.7, glycerol 2.2-2.8, ceruloplasmin 0.06-0.08, L-asparaginic acid 0.04-0.06, a solvent with pH 5-7 - the rest. What is described is a method for preparing the coating consisting in the fact that a chitosan weigh is diluted in the solvent at 1000 mg of the weigh to 15 ml of the solvent, mixed and placed in a thermostat at a temperature of 37-42°C for 1-2 hours. The mixture is added with ceruloplasmin diluted in the solvent at 1:10 to form a homogenous hydrogel. L-asparaginic acid is diluted in the solvent pre-heated to 37-40°C and added to the mixture to provide pH of the mixture 5-7. A plasticising agent in the form of glycerol is added in the amount of 2.2-2.8% of total volume of the prepared biomass The prepared biomass is placed into containers to form a uniform layer of the coating 3-5 mm high and to form a film by drying the biomass for 18-24 hours in the thermostat at a temperature of 37-40°C. n EFFECT: wound coating provides the highest clinical effect. n 6 cl, 6 dwg, 2 ex |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2613112-C2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EA-028141-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2694372-C1 |
priorityDate | 2013-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 88.