http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2508254-C1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1455f69a13f91030b0c2c7ff78e3e662 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C6-04 |
filingDate | 2012-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ff714a33d238aeacf2b779a3e4831f2d |
publicationDate | 2014-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2508254-C1 |
titleOfInvention | Mixture for making glaze |
abstract | FIELD: chemistry. n SUBSTANCE: mixture for making glaze contains wt %: kaolin 3.0-5.0; feldspar 12.0-16.0; quartz sand 57.0-58.0; chalk 1.0-2.0; tin oxide 5.0-7.0; zinc oxide 1.0-2.0; barium carbonate 1.0-2.0; cobalt sulphate 1.0-2.0; bone ash 12.0-16.0. The glaze has thermal stability of (heating at 100°C in boiling water - cooling to 15°C in water) 20 cycles. Parts of mixture for making glare are melted of temperature 1430 - 1450°C. n EFFECT: high thermal stability of the glaze. n 1 tbl |
priorityDate | 2012-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |