http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2492438-C1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_edc4c223a6f1ce1b83896ca98a86393d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01L1-00 |
filingDate | 2012-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2013-09-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cbf022c2ccc1e34e166f2f6f56b4ff14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9808760c41653b6fe21231321a0fa11e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c0337b39fc624ccaacee89af3162c7b7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e61913885e11d3be35038aadd8a83b68 |
publicationDate | 2013-09-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2492438-C1 |
titleOfInvention | Brittle coating for caramel-based deformation and stress analysis |
abstract | FIELD: measurement technology. n SUBSTANCE: invention relates to determination of the stress-strain state of metal structures of high-risk facilities in the oil, gas and chemical industry, transportation systems and oil and gas processing using brittle strain-sensitive coatings, which enables to obtain a clear picture of the highest stress concentration and obtain data for evaluating strength of potentially hazardous structures. The brittle coating for deformation and stress analysis is made from a mixture containing water and sugar, with the following ratio of components, wt %: water 65-75, sugar 25-35. n EFFECT: reduced harmful effect on the environment. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2592889-C1 |
priorityDate | 2012-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 23.