http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2479503-C1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1455f69a13f91030b0c2c7ff78e3e662 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C6-04 |
filingDate | 2011-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2013-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ff714a33d238aeacf2b779a3e4831f2d |
publicationDate | 2013-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2479503-C1 |
titleOfInvention | Glaze |
abstract | FIELD: chemistry. n SUBSTANCE: invention relates to the industry of construction materials and glaze compositions for applying on ceramic tiles and bricks. The glaze contains the following, pts.wt: yellow lead 29-31; ground glass 10-12; ground malachite 6-8; quartz sand 10-12; bone ash 6-8. The glaze has frost resistance of not less than 100 cycles. The glaze is molten at temperature of 1430-1490°C and fired at 1120-1150°C. n EFFECT: high frost resistance of the glaze. |