http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2470034-C2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b8be6a6c990669567cc455d32b00535e |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D167-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F299-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F4-654 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F299-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F299-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-28 |
filingDate | 2008-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2012-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e4bb747a0da403372ffff06a6f7e32e3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6ee8dad751e57df5e403b413e66e4257 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e32d489e04ed2aa367af11a674005112 |
publicationDate | 2012-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2470034-C2 |
titleOfInvention | Activating solution |
abstract | FIELD: chemistry. n SUBSTANCE: invention relates to activating solutions containing a complexing agent. Described is use of the activating solution for curing unsaturated polyester (UP) resin or acrylic resin, said solution containing a complexing agent selected from a group consisting of complexing agents having a nitrogen atom and a hydroxyl group, and bipyridine, a metal salt selected from a group consisting of a transition metal, magnesium and lithium, and optionally a solvent, wherein if the complexing agent has a nitrogen atom and a hydroxyl group, the amount of the complexing agent in the activating solution is at least 5 wt % with respect to the total weight of the activating solution, the amount of the solvent is less than 50 wt % and the amount of diethylene glycol as a solvent is less than 25 wt % with respect to the total weight of the activating solution. Described is an activating solution containing a complexing agent selected from a group consisting of monoethanolamine, diethanolamine, triethanolamine, dimethylaminoethanol, and bipyridine, a metal salt selected from a group consisting of a transition metal, magnesium and lithium, and a solvent, wherein if the complexing agent has a nitrogen atom and a hydroxyl group, the amount of the complexing agent in the activating solution is at least 5 wt % with respect to the total weight of the activating solution, the amount of the solvent is less than 50 wt % and the amount of diethylene glycol as a solvent is less than 25 wt % with respect to the total weight of the activating solution. n EFFECT: wider range of activating solutions having improved characteristics, particularly for curing unsaturated polyester (UP) resin or acrylic resin. n 17 cl, 12 tbl, 27 ex |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2674416-C1 |
priorityDate | 2007-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 144.