http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2455377-C2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6592a85a60c6d74035b952f5f8518922 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C1-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F9-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C29-14 |
filingDate | 2010-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2012-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_979c101ec580cfa317c5fa55a589947d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fac3054fae6aab0eb06371159f804a68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_addaea0dbc07acb5299f6fa4a694c723 |
publicationDate | 2012-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2455377-C2 |
titleOfInvention | Method to produce metal-boride composite powders of molybdene and tungsten |
abstract | FIELD: metallurgy. n SUBSTANCE: molybdenum or tungsten compounds with a boron compound are reduced with metallic magnesium in a molten salt mixture medium of NaCl-NaF (1:1) at a temperature of 800-900°C. The ratio of oxides of molybdenum or tungsten compound with boron is maintained at 1:2.5 of mass fraction, and the ratio of molybdenum or tungsten oxides with magnesium is 1:0.45 of mass fraction. n EFFECT: production of composite fine powders of Mo-MoB, W-WB with a low content of impurities at low temperatures is provided. n 2 cl, 2 ex |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2661164-C1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2692543-C1 |
priorityDate | 2010-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 37.