http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2418682-C2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_595e8914cb6262c7e52b0fecbfc1a965 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31522 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2666-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31757 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31855 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J123-0815 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-32 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J151-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J123-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-04 |
filingDate | 2006-05-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2011-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4b34ae967816e7ece4e8af2178d21726 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b6641742cf62daaae405ec8e836976ba http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dfe8a0bca240f21ad38c99c86a360efe http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_64cf091495dc3ba7634cd16163b735ba |
publicationDate | 2011-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2418682-C2 |
titleOfInvention | Binder for co-extrusion of co-grafted polyethylene and polypropylene, diluted in ungrafted polyethylene |
abstract | FIELD: chemistry. n SUBSTANCE: invention relates to binder for co-extrusion based on a mixture of co-grafted polyolefins, as well as a multilayer structure containing the binder. The binder contains a mixture of at least homo- or copolymer of ethylene (A1), having density 0.940-0.980 g/cm 3 , and at least one copolymer of propylene (B) containing at least 51 wt % propylene. (Co)polymers of the said mixture are co-grafted with a functional monomer selected from carboxylic acids and their derivatives. The degree of graft polymerisation of the extrusion binder is more than 0.05 wt % and less than 0.5 wt % of the total weight of the said binder. The mixture is possibly diluted in at least a homo- or copolymer of ungrafted ethylene (A2). Said binder has density of 0.940-0.980 g/cm 3 . n EFFECT: disclosed binder has sufficient fluidity, high resistance to peeling of layers at temperature higher than 80°C, and is meant for use in a multilayer structure for protecting metal surfaces and for making packaging, rigid hollow housings, particularly bubbles or bottles, or flexible reservoirs, as well as multilayer films. n 13 cl, 2 tbl, 4 ex |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2562267-C1 |
priorityDate | 2005-05-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |