http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2392972-C2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_08edeea18d6232ad06e326e416b529dd |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L15-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K31-79 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K9-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L17-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K33-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L5-08 |
filingDate | 2008-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2010-06-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bc073f297cd05d0531b49ea27de7df8b |
publicationDate | 2010-06-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2392972-C2 |
titleOfInvention | Method of obtaining polysaccharide material |
abstract | FIELD: chemistry. n SUBSTANCE: invention relates to a method of obtaining polysaccharide fibre for making materials, specifically for making surgical suture materials absorbable in a human and a mammal body, absorbable and non-absorbable dressing material and absorbable textile matrix materials. The method is characterised by that 2.4-4.0 wt % solution of polysaccharide in dimethylacetamide which contains 4.56-10.00 wt % lithium chloride is mixed with 1.0-5.0 wt % poly-N-vinylpyrrolidone with molecular weight of 8-35 kDa or a metallopolymer complex - fine-grained silver stabilised by poly-N-vinylpyrrolidone in such an amount that, content of fine-grained silver relative polysaccharide dissolved in spinning solution ranges from 0.07 to 0.87 wt %. Mass ratio of polysaccharide: metallopolymer complex equals 88.0-99.0:1.0-12 wt %. The mixture is intensely stirred, held, filtered, degassed and the obtained spinning solution is extruded at room temperature into an alcohol deposition tank in form of water-soluble aliphatic C 2 and C 3 alcohols. The fibre is then processed in plastification and washing tanks and dried. n EFFECT: obtaining fibre with good deformation and strength properties. n 1 dwg, 4 tbl, 29 ex |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2621114-C2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2639770-C2 |
priorityDate | 2008-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links