http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2354743-C2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cbeb0bfbccaf87e52b01dbe811bcbf39 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C8-38 |
filingDate | 2007-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2009-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_10019eddfe34507da1bd517ed89fe92f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aaf1c8563583a182b4eda25b6ef7cc05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1f47c6f69561871ce6fe1fc408de980f |
publicationDate | 2009-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2354743-C2 |
titleOfInvention | Application method of thin-film coating on metal works |
abstract | FIELD: processes. n SUBSTANCE: invention can be used with manufacturing of cutting tools, products of triboengineering function, heavy loaded machinery and mechanisms. Coating is applied by means of displacement of low-temperature plasma stream, containing carbon, silicon, hydrogen, nitrogen, oxygen and argon, lengthwise the product surface. Products are preheated up to the temperature 50-100°C. Displacement of low-temperature plasma stream is implemented at a rate of 3-150 mm/s. Total time of coating is assigned depending on processing surface area and coating thickness. n EFFECT: ensured by coating of thin-film wear-resistant coating with defined thickness with high adhesion to the basis it is achieved useful increase of product's service durability by increased reproducibility. n 4 tbl |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2548847-C2 |
priorityDate | 2007-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 25.