http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2352027-C2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_506a6d4c5eb03c3c0718ae53e8265a2a http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c16d2144a81bfa32a665dca1e93c3d37 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K71-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K50-15 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K50-17 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L51-50 |
filingDate | 2007-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2009-04-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d79b2df801d92c49c2095c4f588f27f6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d097a99098fe6dd43174a9cd18507ef5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_374e45a0f2fea18c4e7481d915d97390 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_12e9b83b8a1a42e592f48f06be4ab58a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2c97b298487e3fcdc21a6aa6ae988513 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e9984c6972e484380464ab3c65881f27 |
publicationDate | 2009-04-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2352027-C2 |
titleOfInvention | Method of injector coating for polymer electroluminescent diodes |
abstract | FIELD: chemistry. n SUBSTANCE: there is disclosed method of injector polyaniline coating on the surface of transparent conductive oxide or metal layer on transparent substrate for the polymer electroluminescent diode, characterised that polyaniline coating is ensured with electrochemical synthesis of polyaniline from aniline solution being in contact with transparent conductive oxide or metal layer. Invention prevents softening ensured by prevented current spreading along the polyaniline layer, as well as by simplified procedure of polyaniline coating; homogeneous coating of easily controlled thickness; polyaniline coating of high continuity without through holes; with required pixel array addressing without additional polymer layers of reduced conductivity. n EFFECT: simplified and cheap making polymeric electroluminescent diodes. n 10 cl, 2 dwg |