http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2258765-C2
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-265 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-264 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-13 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-08 |
filingDate | 2002-02-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2005-08-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dac5db4b4c3ceef11652cba1dbbefda9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b9766e7273b30b54244f0e8529293220 |
publicationDate | 2005-08-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2258765-C2 |
titleOfInvention | Surface-treated steel material, method of its production and a liquid for a chemical conversion treatment |
abstract | FIELD: methods of production of surface-treated steel materials and liquids for the steel materials chemical conversion treatment. n SUBSTANCE: the invention is dealt with a method of chemical conversion treatment of a steel material, which is produced with usage of a method of a surface treatment and a liquid for the treatment, in particular, to surface-treated material having an excellent positive resistance to a galling. The surface-treated steel material contains a steel material and a chemical conversion film. At that the chemical conversion film contains potassium in amount of 0.1-1000 mg/m 2 and has a thickness within the range of 5-48 microns or within the range from exceeding 48 up to 50 microns. The method provides for the chemical conversion treatment realization on a surface of a steel material with utilization of a liquid containing zinc and phosphoric acid or manganese and phosphoric acid plus potassium. The invention allows to create a liquid, which due to addition of potassium forms a stable film of a phosphate type even on a steel, containing: chromium 0.5-13.0 %. n EFFECT: the invention ensures creation of a liquid, which forms a stable film of a phosphate type even on a steel, contai ning some % of chromium. n 15 cl, 4 ex, 5 tbl, 1 dwg |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7850792-B2 |
priorityDate | 2001-02-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 55.