http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2251560-C2
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-17 |
filingDate | 2003-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2005-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bd4a0a0f4adc15c7ae9d7509a2a78835 |
publicationDate | 2005-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2251560-C2 |
titleOfInvention | Epoxyde composition and method for production the same |
abstract | FIELD: chemistry, in particular organic polymeric compounds and compositions. n SUBSTANCE: claimed composition contains epoxy-dianic resin with molecular weight at most 390, aliphatic epoxy resin, and triethyleneamin as curing agent. Composition is obtained by addition of 5-10 mass pts of aliphatic epoxy resin to 100 mass pts of epoxy-dianic resin and mixture is blended to obtain homogeneous mass. Then 13-14 mass pts of triethyleneamin as reduced to 100 mass pts of resin is admixed and cured at room temperature for one day followed by auxiliary curing at 100-120°C for 3-5 h. Composition of present invention is useful in production of heat resistant polymeric constructional materials for aerospace and machine industry. n EFFECT: epoxy compositions with improved strength and heat resistance. n 2 cl, 3 tbl, 3 ex |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2528681-C2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2696623-C1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2623774-C1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2606614-C1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2603362-C1 |
priorityDate | 2003-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 28.