Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_464eb9068823683b5a4a63aa3cb13553 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2327-06 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-02 |
filingDate |
1990-11-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1998-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_199bcf5e60806cab55873511e81356e1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_35e7156206967edf7b9ef0e995f90e7c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d429c5e2296102b117dc36b2e8693353 |
publicationDate |
1998-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
RU-2105775-C1 |
titleOfInvention |
Method of preparing cross-linked plastic foam |
abstract |
FIELD: chemical industry, particularly preparation of cross- linked foamed polymers. SUBSTANCE: claimed method comprises preparing cross-linked foamed vinyl chloride- based copolymer prepared by polymerization vinyl chloride and glycedyl (epoxy) containing 0.05-30% monomer and, optionally, other monomer by mixing said monomers with foaming and cross-linking agent during heating operation. Decomposition products are chemically active to epoxy groups of copolymer. EFFECT: more efficient preparation method. 9 cl, 9 tbl |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2727862-C2 |
priorityDate |
1989-12-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |