http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2048975-C1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c5889f6f5b0ec8c039c3e05c67ea70b4 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F9-04 |
filingDate | 1990-02-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1995-11-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_633fb86f6ceb6141342566ef87236bac http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e7bf1fa81f1b12b9cd336b716e01eac6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9f6d27a0a3b19224e3e17cd4ed49af10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_62c5c8de6daf049eb0a629ef8ae81538 |
publicationDate | 1995-11-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2048975-C1 |
titleOfInvention | Method of producing chrome boride powder |
abstract | FIELD: metallurgy. SUBSTANCE: process of chrome boride smelting in ore-thermic electric furnace is carried out using the charge in which the ratio of diboron trioxide to chrome sesquioxide is 0.46-0.8, and the ratio of carbon to the total content of boron and chrome oxides is 0.41-0.55. Method provides producing monophase solid liquid boron-chrome. EFFECT: improved method of chrome boride producing. 3 tbl |