http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2026324-C1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e8c9878306b6832810b95d93395af670 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L97-02 |
filingDate | 1991-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1995-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f1aeedea8f1ed45af88e81abc3432f4c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_85f83cbdfd229bb072b5546e76786822 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_553ff104a2faaec9b34706dea0537e77 |
publicationDate | 1995-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-2026324-C1 |
titleOfInvention | Molded polymeric composition |
abstract | FIELD: building industry. SUBSTANCE: the composition comprises (wt %): 10-14 carbamido or a phenol formaldehyde binder and a filler, the balance. The filler comprises 43-45 wt % wood chip and 43-45 wt % wood fiber. The specimens are pressed at 168-175 C 6 MPa and 0.5-0.8 mm of the article thickness. The properties of the specimens: the density 600-800 kg/m 3 ; the ultimate bending strength 10-60 MPa; the swelling 10-15%. EFFECT: improved properties of the binder. 2 tbl |