http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2015103145-A

Outgoing Links

Predicate Object
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2219-00761
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-92
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-762
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J8-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B9-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-01
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J19-0066
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J19-18
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F36-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F36-08
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F36-04
filingDate 2013-07-01-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationDate 2016-08-20-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber RU-2015103145-A
titleOfInvention METHOD FOR CONTINUOUS SYNTHESIS OF DIENE ELASTOMER
abstract 1. A method for the continuous synthesis of a diene elastomer, characterized in that it comprises the following simultaneous steps: a) continuously introducing into the polymerization reactor equipped with a gas phase and equipped with at least one mixing means and a discharge device, at least: i. one or more monomers to be polymerized, of which at least one monomer is a conjugated diene, and ii. from 0% to 70 wt.% organic solvent, based on the total weight of the monomers and solvent; b) continuous polymerization of the monomer or monomers, c) stirring the polymerization medium by continuously moving at least one stirring means around the axis of rotation, d) continuous discharge the elastomeric mass at the exit from the polymerization step, e) continuously feeding the unloaded elastomeric mass to the cutting device and cutting it into particles, f) removing solvent from the particles of the elastomeric mass; and g) removing the diene elastomer and particles obtained in the previous step, characterized in that: (1) the degree of conversion is at least 60% within the first third of the reaction volume of the polymerization reactor, and (2) the standard deviation of the distribution function over the residence time in the polymerization reactor is greater than the average time stay divided by 2√3.2. A method for the continuous synthesis of a diene elastomer according to claim 1, characterized in that the degree of conversion is at least 80% within the first third of the reaction volume of the polymerization reactor. The method of continuous synthesis of diene elastomer according to paragraphs. 1 or 2, characterized in that the standard deviation of the distribution function over
priorityDate 2012-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID6557
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID407043279
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID458392451
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID7845
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID456171974
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419547008

Total number of triples: 26.