http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-1812198-C
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_32d40893c0529c17e8d41ea7f1173a5e |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D127-06 |
filingDate | 1990-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1993-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3fca2cbf29bf333bd2a1fadffb9a1f3a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b810bd06cdc1c53af873a686cee5c380 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_22f4e62de5fe8ee710824581c7863e51 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cf3ae8f417ee256f52e8a1a750a54504 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8772c33d778da070cfd2729cc95f91b6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c74b3950daf140d8a3e6fcfc2753852e |
publicationDate | 1993-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-1812198-C |
titleOfInvention | Polymeric binder |
abstract | The inventive binder contains wastes of polyvinyl chloride (PVC) 4.3-4.9 wt.%, Waste acrylonitrile butadiene styrene plastic (ABS) 4.3-4.9 wt.% Copolymer of piperylene with styrene 3.0-3, 4 wt.%, Hexachlorocyclopentadiene 0.4-0.6 wt.%, Cyclohexanone - the rest. Wastes from PVC, ABS plastic, and the styrene copolymer are dissolved in cyclohexanone in a water bath at 85-90 ° C. The mass is cooled to 18-23 ° C and hexachlorocyclopentadiene soluble in cyclohexanone is added, cyclohexanone is added to viscosity B3-4. Characteristics of the composition: adhesive strength 2 points, water resistance 10.9-11.6 kN / m. corrosion resistance 0.95-0.98. 2 tab. |