http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-1812186-C
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0b30649510fe45558ba7194be65bb531 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G101-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-18 |
filingDate | 1990-12-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1993-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8881ec437eaafdf50c6c994d1a213bb6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_66a99c436e51f9bc5e06700d34ad5c03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c0549b6ce39501da33861043a3010ff5 |
publicationDate | 1993-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RU-1812186-C |
titleOfInvention | Method of polyisocyanurate foam plastic preparing |
abstract | Usage: in construction, automotive and aircraft engineering, SUMMARY OF THE INVENTION: Quaternary ammonium salt of the formula: OOCCH3 with m-sngsngon. 1 2 where RI is H, alkyl, RZ is epoxyalkyl in an amount of 8-10 parts by weight mixed with 18 parts by weight of hydroxypropylated xylitol; 13-17 parts by weight are added. trichlorofluorristane is stirred, 15 parts by weight are added. trichloroethyl phosphate and 100 parts by weight of polyisocyanate are stirred, the mixture is poured into a heated mold, after 5 minutes the block is removed from the mold and subjected to further processing at 50-60 ° C for 0.8-1.0 hours. Receive non-combustible penrpolyisocyanurate with an apparent density of 33-46 kg / m3, a compressive strength of 1.88-2.54 kgf / cm. 1 tab. |
priorityDate | 1990-12-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 23.