http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RO-126206-A2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_18446203c3c69721cc4ed7f11a72e156 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_986c7cf3645ddaee26b5b2ce06b58ea2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L29-04 |
filingDate | 2009-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9b2c71da8975dce40b1fcf00a83b7cd8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b453669e2a0a977e456c6b23d35ce46d |
publicationDate | 2011-04-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | RO-126206-A2 |
titleOfInvention | PROCEDURE FOR OBTAINING A FIBER LIQUID AND THIS LICENSE OBTAINED |
abstract | The invention relates to a process for obtaining a polymeric binder for impregnating mineral fibers. The process according to the invention consists in mixing, with stirring, 2 ... 20 parts by weight of acetalized polyvinyl alcohol to a degree of 18 ... 22% to 80 parts by weight of maleic styrene-maleic anhydride terpolymer-acrylate functionalized with polyols or hydroxylamines, up to 80 parts by weight of acrylic acid-acrylonitrile copolymer, water to a solids content of 35-40% and based on the solids content of 1 ... 3% plasticizer, up to 1% stabilizer, resulting in a product in the form of a yellowish-red to reddish-brown aqueous solution with a pH in the range of 5 ... 7 and a Dyne bucket viscosity with 8 mm of 8 ... 144 s . |