http://rdf.ncbi.nlm.nih.gov/pubchem/patent/PL-403635-A1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b49b25798cc9813e3f4a0fbe099b95ab
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23P15-16
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F15C5-00
filingDate 2013-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6479eb7e5f837b613278bea47c6339b4
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5940a88bbf34d75ac179e9194fa0e3e8
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d8917944631706e08054cb75d44f5144
publicationDate 2014-07-21-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber PL-403635-A1
titleOfInvention Production method of ceramic electromagnetic microvalve and ceramic electromagnetic microvalve
abstract The subject of the invention is a method of manufacturing a ceramic solenoid valve, which consists in the fact that at least one layer of the coil (WC) is cut from the raw film, on which metallization is applied by means of screen printing or photo-definable forming an induction coil (CW) and electric grommets are made, afterwards the shapes are cut from the foil and the layers of the system are ripped, with at least one separating layer (WS) being the bottom for the microflow channel (KM), one channel layer (WK) in which the microflow channel (KM) is made , one middle layer (WZ), in which the inlet / outlet holes and valve seat holes (OG) are made, one layer of the valve seat (WG), in which the valve seat (GN), the valve seat hole (OG) and the holes are cut inlet / outlet, one spacer layer (WD), in which the valve hole and inlet / outlet holes are cut, after which the layers are laminated, and then it fires during multi-stage thermal treatment, after which a distance layer (WD) is applied by screen printing with an enamel layer (SZ) and fired for 60 minutes, with the temperature rising from ambient temperature to 850 ° C, and then a membrane (PD) is made ), pouring PDMS material into the mold and baking at 70 ° C for at least 120 minutes, the membrane and the body are plasma modified and connected to the body surface by pressure, after which a magnet (MG) is attached to the membrane (PD). The subject of the application is also a ceramic electromagnetic micro valve.
priorityDate 2013-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID24705
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID414028195

Total number of triples: 15.