http://rdf.ncbi.nlm.nih.gov/pubchem/patent/PL-398788-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_246cac906e262d5b3278c85c9522d9ee |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B14-18 |
filingDate | 2012-04-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0263b694aa1a0d6e5a6771490a4934c7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d55a336f727be0b72d9124467e72addd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0ad6fd64014e5aa4ac4b554be8ebf031 |
publicationDate | 2013-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | PL-398788-A1 |
titleOfInvention | Production method of perlite plastic |
abstract | The method of producing perlite plastic by the method of thickening and curing a mixture made of expanded perlite and a binder used in the form of aqueous alkaline earth metal silicates, consists in the fact that the composition obtained by mixing the expanded perlite with a binder consisting of an aqueous colloidal silicon dioxide solution is subjected to thickening and drying. , preferably a silicic acid sol with the optional addition of sodium and / or potassium water glass, the proportion of the individual components being: - expanded perlite from 1 to 99% by weight, - colloidal aqueous silicon dioxide solution from 1 to 90% by weight, - glass aqueous sodium and / or potassium from 0 to 50% by weight, - water from 1 to 95% by weight |
priorityDate | 2012-04-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |