http://rdf.ncbi.nlm.nih.gov/pubchem/patent/PL-197240-B1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d1d1d1c9a6df2ff5ec6410fbae27965e
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F23G5-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B09B3-40
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F23G7-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B12-00
filingDate 2001-11-21-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8fd5562e757ea8a537941258edc83862
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_86d07fb1f1ea50c10211845abb0ab926
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_30dcede0f750695caff15a57195ecea0
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fccc607d4f43f07e18d79a3724902ba2
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a07e28c2ff0a736f42615babce5eee61
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b05afb1e4f79c7a57d5ce13d80199db1
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a3fcbe4e1c4a7fac983831caa6e971d8
publicationDate 2008-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber PL-197240-B1
titleOfInvention Method of liquidation of processed organic waste by combustion in a rotary cement kiln
abstract The proposed liquidation method of treated organic waste, in particular meat and bone meals, waste fats and another treated veterinary waste of animal origin, by incineration thereof in rotary cement kiln when burning cement is carried out in such a manner that treated organic waste with maximum moisture content of 50 percent, minimum heating value of 11 MJ.kge-1 and with formation of 50 percent by weight of ash, at the most, is added in a rotary cement kiln as a portion of the total amount of fuel either directly into the flame via a main burner and/or via a calcining burner and/or via an auxiliary burner, and/or the treated organic waste is added into said rotary cement kiln hot portion with temperatures above 1400 degC, whereby such amount of the treated organic waste is added into the rotary cement kiln, which evolves by its burning up to 90 percent of heat energy needful for achieving effective temperature for cement burning and simultaneously the amount of the treated organic waste is controlled to maintain amount of phosphorus oxide, expressed as Pi2Oi5 in clinker below the level of 2 percent. This means that the added treated organic waste burns in the kiln under oxidation kiln atmosphere in excess of combustion air and under generation of non-toxic combustion products and ash. Heat energy evolved by this burning is thus employed for effective cement burning, whereby the non-toxic combustion products are partially caught during counter-current cement burning on the ground raw material mixture and on clinker being just formed, and ash arising by incineration of the treated organic waste containing bones reacts quantitatively with clinker mass. Phosphorus oxide, analytically expressed as Pi2Oi5 exhibits in amounts up to 2 percent a mineralizing effect on formation of clinker phases.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/PL-422538-A1
priorityDate 2001-02-19-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID86715555
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID140772
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID451876530
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419520343
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID123290
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID415844527

Total number of triples: 27.