http://rdf.ncbi.nlm.nih.gov/pubchem/patent/PE-20081241-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_28ccea763a4fbc603dad9a691d6c8da4 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B30-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B1-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B15-0017 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B15-001 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B1-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B1-00 |
filingDate | 2008-01-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c3a64fc38e2ea60b1f210b2ed9f3a647 |
publicationDate | 2008-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | PE-20081241-A1 |
titleOfInvention | PROCEDURE FOR OBTAINING COPPER FROM MINES OR CONCENTRATES OF ARSENIC SULFIDE MINES AND / OR ANTIMONY SULFIDE CONTAINING COPPER |
abstract | WHERE THE PROCEDURE INCLUDES: a) TRANSFORMATION OF MINES OR CONCENTRATES OF MINES, BY REACTION IN AN INERT ATMOSPHERE WITH SULFUR FROM 300 ° C TO 600 ° C DURING A TIME BETWEEN 5 MINUTES AND 24 HOURS; b) GRINDING THE REACTION PRODUCT; c) PHYSICAL SEPARATION AT LEAST PARTIAL OF THE ARSENIC AND / OR ANTIMONIUM SULFIDES OBTAINED FROM THE SULFIDES CONTAINING COPPER, THROUGH ELECTROSTATIC, GRAVIMETRIC OR MAGNETIC PROCEDURES, AIR SEPARATION, SELECTION OF SIZES, OR SIZES, OR CLOTHING PROCEDURES. ; AND, d) TREATMENT OF THE SULFIDES CONTAINING SEPARATED COPPER, THROUGH PYROMETALLURGICAL OR HYDROMETALLURGICAL PROCEDURES TO OBTAIN COPPER. (a) IT IS CONTINUOUS, IN A THREE-CHAMBER SYSTEM, AND CARRIED OUT IN A TUBULAR ROTARY OVEN OR FLUIDIZED BED REACTOR. SULFUR IS ADDED STECHOMETRICALLY, SEMIESTECHIOMETRICALLY OR CATALYTICALLY. DURING (a) PRECIOUS METALS ENRICHMENT IS CARRIED OUT IN THE COPPER SULFIDE PHASE. THE MINES OR CONCENTRATES OF MINES ARE SELECTED FROM ENARGITE (Cu3AsS4), TENNANTITA (Cu12As4S13) AND / OR TETRAHEDRITE (Cu12Sb4S13) ASSOCIATED WITH CHALCOPYRITE (CuFeS2), BORNITE (Cu5FeSEN, CALSCUBANITE (Cu5FeS4), CUBANITE (Cu5FeS4), CUBANITE (Cu5FeS4), CUBANITE5 ) AND / OR COVELINA (CuS) |