http://rdf.ncbi.nlm.nih.gov/pubchem/patent/NO-20004101-L
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9f66c116b33583a727509c5af6925fa6 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-54 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G23-0532 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B34-1236 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B34-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G23-053 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C1-36 |
filingDate | 2000-08-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9b8a90fe601abbd975f03eda8fb2ac38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8232c6cf058b79312cd8c647f9a1a152 |
publicationDate | 2000-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | NO-20004101-L |
titleOfInvention | Process and furnace for the preparation of TiO2 pigment according to the sulfate process |
abstract | A process for the preparation of titanium dioxide by dissolving titanium raw materials with sulfuric acid, preparing a metal sulphate-containing titanyl sulphate solution, hydrolysing the titanyl sulphate, separating the titanium dioxide hydrate from metal sulphate-containing sulfuric acid by filtration, optionally bleaching the titanium dioxide anhydride solution and doping chemicals and titanium dioxide nuclei, characterized in that the sulphate-containing titanium dioxide hydrate is dried in a dryer at temperatures from 90 to 400 ° C, preferably 90 to 200 ° C, particularly preferably 90 to 150 ° C, and that the titanium dioxide hydrate dust is separated from the dryer exhaust gas by filtration. the dried titanium dioxide hydrate is calcined in a rotary kiln directly heated with flue gases at temperatures in the range from 800 to 1100 ° C (solids temperature) and the exhaust gas is dust cleaned and desulfurized. Calcination furnace for the production of titanium dioxide from dried sulphate-containing titanium dioxide hydrate in the form of a rotary kiln with a length-diameter ratio in the range 5 to 10. |
priorityDate | 1998-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 28.