http://rdf.ncbi.nlm.nih.gov/pubchem/patent/NL-7906877-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_caab3b41d140ac049cc044a24ba37217 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F110-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F110-02 |
filingDate | 1979-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 1980-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | NL-7906877-A |
titleOfInvention | METHOD FOR PREPARING POLYETHENE WITH ULTRA-HIGH MOLECULAR WEIGHT |
abstract | Polyethylene or ultra high mol. wt. is prepd. by contacting ethylene with a catalyst, contg. (a) a heat-activated organo-phosphoryl-Cr cpd. on (b) Al2O3 with pore vol. 0.3-2.2 (1.2-2)cc/g as carrier. The cpd. (a) is obtd. by reacting CrO3 with (RO)3PO(I) or (RO)2P(OH), (II) where R is (cyclo)alkyl, aralkyl, aryl or H and is not 1 R is nor H. Polyethylene has mol. wt. 1,000,000 to >6,000,000 (is not 2,000,000), and has improved mechanical strength. |
priorityDate | 1978-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 54.