abstract |
The invention relates to an article for personal care; the article comprises a substrate; and a personal care composition disposed on the substrate, the coating of the personal care composition forms a coated region of the substrate, wherein the personal care composition has a yield point of 10 Pa to 2000 Pa, preferably, from 30 Pa to 1200 Pa, more preferably, from 45 Pa to 500 Pa and, even more preferably, from 60 Pa to 300 Pa, determined by means of a controlled effort amplitude sweep; at a frequency of 1 Hz and a temperature of 25 ° C, and wherein the personal care composition is arranged on the substrate in an amount per unit area of the coated region of 0.300 g / cm2 to 0.001 g / cm2, with more preferably, from 0.015 g / cm2 to 0.003 g / cm2, even more preferably, from 0.080 g / cm2 to 0.005 g / cm2 and, even more preferably, from 0.05 9 / cm2 to 0.005 g / cm2. |