http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-980009552-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2401-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2401-061 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D02G3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D02G3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D10-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-86 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-62 |
filingDate | 1996-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 1998-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-980009552-A |
titleOfInvention | Process for producing high melting point polyether ester fiber |
abstract | In the present invention, two polyether esters having different hard segment contents are melt-mixed in a range of 20 to 80% by weight of the hard segment and 20 to 80% of the soft segment, respectively, so that the average hard segment content is 20 To 40% by weight, the polyetherester produced according to the present invention has a melting point higher than that conventionally produced by using a single hard segment, It is also possible to dye under the conditions and has good dye fastness, so that it does not change the strength or kidney recovery rate even after dyeing. |