http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-950025066-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-226 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-16 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 |
filingDate | 1994-02-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 1995-09-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-950025066-A |
titleOfInvention | Master batch composition for injection molding polyolefin resin showing natural stone pattern and polyolefin resin molded article production method using the master batch composition |
abstract | BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a master batch composition applicable to the production of a polyolefin resin molded article exhibiting an outer plate of natural stone pattern such as marble and granite, and a method for producing a polyolefin resin molded article using the master batch composition. Since the pattern is formed after injection molding, the method of applying the pattern is complicated, so that the productivity is low and it is difficult to apply to a complex product. The present invention has a polyolefin resin of 30 to 50 parts by weight, and a polyamide resin of 25 to 45 ° C. 200 parts by weight to 200 parts by weight of the modified polypropylene resin binder and about 2 to 3 parts by weight of a master batch composition for injection-molded polyolefin resins composed of an appropriate amount of pigments, dispersants and preparations and about 2 to 3 parts by weight of the composition. Preparation of Polyolefin Resin Molded Article Injection Molded at ℃ Act as a molded exterior to allow a natural stone pattern may direct. |
priorityDate | 1994-02-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links