titleOfInvention | Styrene-based antistatic thermoplastic resin composition |
abstract | The present invention relates to a thermoplastic resin composition having permanent antistatic properties and having excellent mechanical properties represented by impact strength.n n n It is an object of the present invention to provide a styrene-based thermoplastic resin composition which provides a permanent antistatic property to a styrene-based resin, and prepares an antistatic resin having excellent physical properties and appearance.n n n The present invention is characterized by consisting of 5-50 wt% of (A) poly (alkylene oxide) -based polymer and 50-95 wt% of (B) styrene resin.n n n (A) Poly (alkylene oxide) polymern n n ① 30-90wt% poly (alkylene oxide) amine with molecular weight 200-10000n n n ② 5-30 wt% of ethylene glycidyl methacrylate with glycidyl methacrylate of 5-50 wt%n n n ③ 5-40wt% polycaprolactone with molecular weight of 5000-70,000n n n (B) styrene resinn n n ① 20-90 wt% of polymer obtained by graft polymerization of 95-20 wt% of aromatic vinyl monomer and vinyl cyanide mixture to 5-80 wt% of rubber copolymern n n ② 10-80 wt% of a polymer obtained by mixing 40-10 wt% of an aromatic vinyl monomer and 60-10 wt% of a vinyl cyanide monomer and 0-40 wt% of a polymerizable other vinyl monomer. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100492806-B1 |
priorityDate | 1993-06-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 19.