http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-930006089-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 |
filingDate | 1992-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 1993-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-930006089-A |
titleOfInvention | Polyethylene blend |
abstract | ?? which is composed of the following (a), (b) Blends; (a) 10 to 80 weight percent low molecular weight polyethylene resin having a density of at least 0.94 grams per cubic centimeter, a melt index of at least 25 grams per 10 minutes, and a heterogeneity index of 2 to 12, and (b) no more than 0.955 grams per cubic centimeter 20 to 90 weight percent high molecular weight ethylene copolymer having a density of, a high load melt index of 2 to 10 grams per 10 minutes, and a heterogeneity index of 2 to 10; The composition of matter then has a melt index of at least 0.05 grams per 10 minutes. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100387648-B1 |
priorityDate | 1991-09-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 32.