abstract |
The laminate of the present invention has a support and a translucent resin layer disposed on the surface thereof so that peeling is possible. When the coefficient of thermal expansion of the support is CTE1 and the coefficient of thermal expansion of the translucent resin layer is CTE2, the ratio CTE2/CTE1 of the coefficient of thermal expansion is 2 to 5.5, and the coefficient of thermal expansion CTE of the laminate is 10 to 30 ppm/K. |