Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b0f9e1dbaa34bf69e9b0a8247c4abfe7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8205ec6ee1cd95eb60a03826535bad97 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-0008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-26 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E04G21-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B40-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-085 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B111-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B103-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B111-72 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B40-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E04G21-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-08 |
filingDate |
2020-07-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_35529a7702f8ef5af72e681e1b6b3ed1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_15f56d7f287257f9223366efd3f51887 |
publicationDate |
2022-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20220050142-A |
titleOfInvention |
Cement-based grout material and its construction method |
abstract |
Cement-based grout material that does not freeze even in an environment where the outside temperature is likely to be -5℃ or lower, and does not require large-scale facilities such as a curing mold or fuel to maintain the curing temperature, and ensure quality. to provide. Lithium nitrite is added to the cement-based grout material containing cement, water, and an admixture. By setting the weight ratio of lithium nitrite to the weight of cement to be 3 to 10% by weight, large-scale facilities for maintaining the curing temperature or fuel for heating are used even under the construction environment where the outside temperature at the initial stage of construction is -5°C. It is possible to prevent freezing of the grout material and ensure quality. If the weight ratio of lithium nitrite is 4.5 to 8% by weight, even under a construction environment where the outside temperature at the initial stage of construction is -10°C, large-scale facilities for maintaining the curing temperature or fuel for supplying heat are not used. By preventing freezing, quality can be secured. |