http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20210134721-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2650-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-4012 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L27-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L71-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L71-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-02 |
filingDate | 2020-03-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-11-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20210134721-A |
titleOfInvention | Resin composition and molded article |
abstract | A resin composition capable of producing a molded article having excellent tensile elongation at break without causing surface peeling and also excellent in low dielectric constant is provided. A resin composition comprising an aromatic polyether ketone resin (I) and a fluorine-containing copolymer (II), wherein the average dispersed particle diameter r1 of the fluorine-containing copolymer (II) and, according to ASTM D1238, 380° C. under a load of 5000 g and A resin composition characterized in that the ratio r2/r1 of the average dispersed particle diameter r2 of the fluorine-containing copolymer (II) after measuring the melt flow rate by preheating for 5 minutes is 1.60 or less. |
priorityDate | 2019-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 140.